| 项目性能 |
性能子项 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
| 机械性能 |
硬度计硬度 |
邵氏 A, 1 秒 |
ASTM D2240 |
39 |
|
| 拉伸应力 |
300%应变, 25℃ |
ASTM D412 |
1.65 |
MPa |
| 抗张强度 |
屈服, 25℃ |
ASTM D412 |
32.4 |
MPa |
| 伸长率 |
断裂, 25℃ |
ASTM D412 |
1400 |
% |
| 应力松弛 |
Peak Force @ 200% strain (A): 23℃, 889.0 µm |
|
1.10 |
MPa |
| 应力松弛 |
Peak Force @ 500% strain: 23℃, 889.0 µm |
|
2.28 |
MPa |
| 应力松弛 |
Ratio (A:B): 23℃, 889.0 µm |
|
2.60 |
|
| 应力松弛 |
Relaxation @ 200% strain: 23℃, 889.0 µm |
|
6.0 |
% |
| 应力松弛 |
Set after 500% strain: 23℃, 889.0 µm |
|
16 |
% |
| 应力松弛 |
Unload @ 50% strain (B): 23℃ 889.0 µm |
|
0.414 |
MPa |
| 补充信息 |
Diblock Content |
|
Internal Method |
< 1.0 |
wt% |
| 挥发性 |
|
Internal Method |
0.2 |
wt% |
| 物理性能 |
比重 |
|
ASTM D792 |
0.928 |
g/cm3 |
| 熔流率 |
200℃/5.0kg |
ASTM D1238 |
12 |
g/10 min |
| 溶液粘度 |
|
ASTM D2196 |
880 |
mPa·s |
| Styrene Content |
|
Internal Method |
18.0 |
wt% |
| 灰含量 |
|
ASTM D1416 |
0.3 |
wt% |